Cold Forming
In the manufacture of small parts using cross-cutting or cold heading machines, high scrap rates often result from defective starting material. Testing the initial material and cutting out the defective sections of wire only leads to multiple short coils that increase changeover times and production costs for the parts manufacturer. Instead, the solution is to inspect the wire immediately before it is cut into small parts. Defective or unfinished parts are then automatically sorted as scrap and are not processed further. Thus, excessive costs of pre-tested initial material can be avoided.
Prüftechnik's Eddychek 5 has been specially equipped with dedicated software for testing on cold formers. It features full sorting, documentation and networking capabilities.

|
(1) The incoming material is tested for defects by an encircling coil.
(2) The Eddychek 5 evaluates the defects it finds, registers their position, and ... |
|
(3) ... tracks the occurrence through the machine in piece-part increments.
(4) When a defective part reaches the forming exit, the Eddychek 5 then sends a sort signal to the reject mechanism to divert individual parts into a scrap bucket. |
|
|
|